permanent smco magnet/customized sintered smco magnet/cobalt smco magnet
Product Description
SmCo magnet magnets are ideal component sepecially in applications where temperature
changes across a broad range or enviroment is corrossive. The cost of SmCo material is the
most expensive, so SmCo magnet is recommended only when its performance is a high
temperature environment concerned.
The advantages of SmCo Magnet:
SmCo magnet is one kind of rare earth magnet with a high percentage of samarium,
which is relatively stable against temperature change.
SmCo magnet has high energy and excellent coercive force, this material is ideally compact
and suitable to highly efficient machines and components, and widely used in application in
which higher operation temperature, higher corrosion and oxidation resistance are crucial.
SmCo magnet has the best temperature characteristics in rare earth material family.
Shape of SmCo Magnet: Disc, Ring, Block, Segment, Cylinder, Trapezoid, Customized Design
changes across a broad range or enviroment is corrossive. The cost of SmCo material is the
most expensive, so SmCo magnet is recommended only when its performance is a high
temperature environment concerned.
The advantages of SmCo Magnet:
SmCo magnet is one kind of rare earth magnet with a high percentage of samarium,
which is relatively stable against temperature change.
SmCo magnet has high energy and excellent coercive force, this material is ideally compact
and suitable to highly efficient machines and components, and widely used in application in
which higher operation temperature, higher corrosion and oxidation resistance are crucial.
SmCo magnet has the best temperature characteristics in rare earth material family.
Shape of SmCo Magnet: Disc, Ring, Block, Segment, Cylinder, Trapezoid, Customized Design
Technical Data Sheet
permanent smco magnet
Curie Temp. | Tc | °C | 800-850 | Coeff. Of thermal expansion | C // | 1/°C | ~8×10-5 |
Density | D | g/cm3 | 8.3-8.5 | C⊥ | 1/°C | ~11×10-5 | |
Recoil permeability | rec | 1.00-1.05 | Regidity Strength | N/m2 | ~1.5×108 | ||
Max.working Temp. | Tmax | °C | 350 | Compress Strength | N/m2 | ~8×108 | |
Electrical Resistivity | ΩCm | ~8.6×10-5 | Tensile Strength | N/m2 | ~3.5×107 | ||
Vickers Hardness | Hv | 500-600 | Young’s modulus | N/m2 | ~1.2×1011 | ||
Thermal Conduct Rate | W/mK | ~12 | Magnetization field Ha | kA/m | ≥1600 |